Home Failure Analysis Litigation Support

Litigation Support

MATCO is ideally suited to provide full-service support for litigation in the fields of materials. MATCO’s scientists have decades of experience in both developing and testing materials of almost all kinds, from traditional steels and specialty alloys to ceramics, paints and coatings. MATCO has provided standards-based testing or has developed and defended new protocols where standards don’t exist in the industry.

An example of such a case is in the analysis of an imported ceramic fireplace which was implicated in the burning-down of an expensive home. The question was: did the fireplace fail, starting the fire, or did the fire begin in some other way, causing the fireplace to collapse, shatter and become charred?

This was a complex investigation. The industry that makes these fireplaces has no internal standards. The broken one had to be compared to similar new ones to see if there were materials-related causes for the failure. Petrographic microscopy work showed significant flaws in the fabrication of the fireplace and tell-tale inhomogeneities suggested stress-concentrations that made failure more likely. Scanning microscopy and energy-dispersive x-ray spectroscopy identified the chemistry of those inhomogeneities. It was learned also that the owner had not provided a sand bed in the base of the fireplace to spread the heat from the burning fuel.

In the long run, although a specific opinion could not be provided on the timing of the failure, the preponderance of the evidence suggested both an extremely low grade product and unwise use of that product.

At MATCO, we specialize in failure analysis and corrosion investigations. We will determine if a failure is caused by inappropriate material selection, design, fabrication or operating conditions. Major corporations that rely on MATCO expertise include US Airways, Allegheny Energy, Follansbee Steel, General Electric, Southern California Edison, Sony Electronics, ABB Power and many more.

Some of the components for failure analysis that we look at in a typical day included mechanical equipment; superheater & boiler tubes; wire cables; pipelines; pressure vessels; forgings; castings; welds/brazes; tools and dies; gears; FRP/PVC pipe; and rebar.

Determination of the root cause of failure of systems or components can be very complex, and may require multidisciplinary testing and analysis. The first requirement for success is having a full-equipped modern laboratory. MATCO’s labs include light and electron microscopy (SEM,AES, TEM), mechanical and corrosion & electrochemical testing, environmental testing, chemical characterization, FTIR, X-ray diffraction, electronic testing, and fracture mechanics/FEA analysis capabilities.

The other half of the battle is having the right staff. MATCO ‘s staff includes experienced PhD-level Metallurgists, FEA analysts, Mechnical Engineers, Materials and Polymer Scientists; Professional Engineers; Chemists; Paint and Coating Specialists; and NACE (National Association of Corrosion Engineers) Certified Corrosion Engineers, Materials Selection/Design, Coatings and Cathodic Protection Specialists. By combining the right equipment with the right staff, rapid and accurate determinations of the causes of failure can be made.

Walter Gretz, Debra Riley and Dr. Zee Discussing a Failure Analysis Project

Finite Element Analysis

The finite element method is a powerful numerical tool for analyzing mechanical components and systems. The representation of a component or system mathematically with finite element, generally involves a discretization of the structure into many small pieces, e.g. small brick-like elements (hence the name of the method).

 

The solution to the equations that govern the behavior of the structure is approximated on each and every brick. The collective effect of all the bricks is taken into account during a step that synthesizes the solutions for each brick to one solution valid for the entire structure. This global solution represents the solution to the equations that govern the structure's behavior. The finite element method provides an accurate tool to predict and evaluate component response, elastic or non-linear plastic, subjected to thermal and structural loads.

Thermal analyses may include convection, conduction, and radiation heat transfer, as well as various thermal transients and thermal shocks. Structural analyses may include all types of constant or cyclic loads, mechanical or thermal, along with non-linearities, such as opening/closing of contact surfaces, friction, and non-linear material behavior.

On-site Inspection & Investigations

Our certified team of inspectors can perform non-destructive testing on project sites to evaluate the integrity of large structures. Our team has performed such analyses nation and worldwide, and will travel to your project site at a moments notice for emergency evaluations. Such large structure evaluations have included off-shore oil platforms, wind power generation towers, concrete domes and stadiums, large underground cooling systems, and large elevated water towers. Our projects have taken us from Aloha Stadium in Hawaii to Alyeska Ski Resort in Alaska; from bridges in Pennsylvania to titanium structures in Tokyo, Japan.

Corrosion Failures

The investigation of corrosion failures can be very complex, and usually requires multidisciplinary testing and analysis to determine the root cause of failure. The end determination must be able to be made with a high degree of certainty to ensure that proper replacement materials are selected and that the most effective corrosion control methods are used. Experience is surely the most important ingredient to look for when choosing a materials firm to handle your corrosion control and failure analysis needs.

Corrosion Engineering & Failure Analysis

Experienced PE, PhD Scientists, NACE Certified in Corrosion, Coating, Design , Materials Selection & Cathodic Protection Specialists who will solve your corrosion problems at both initial design stages and in service. MATCO provides corrosion evaluation and failure analysis investigations for : (a) underground facilities (b) above ground facilities and (c) strcutres in marine environments. MATCO can investigate corrosion or corroso -related failures using state of the art techniques.Reports will be generated detailing corrosion failure causes and recommended means of prevention.

  • Corrosion evaluation, life expectancy determination and cathodic protection of underground pipe lines, water mains, electrical poles and transmission lattices
  • Corrosion mapping, detection of "Hot Spots", cathodic protection of reinforced concrete structures
  • Coating/Paint Investigations
  • Electrochemical EIS , DC and AC Testing - Determination of cathodic protection criteria for non-ferrous alloys and stainless steels
  • On-site Evaluation of tanks and corrosion mitigation by protective coatings and internal or external Cathodic Protection
  • Corrosivity determination of soil, water and determination of corrosion mitigation techniques
  • On-site coating evaluation and selection of coatings for specific corrosive environments by EIS

Electrochemical Corrosion Testing of Three Types of Diffusion Coating

Welding Engineering Services

1. Weld Procedures

MATCO can provide a full-time Welding Engineer at your facility to develop and document required welding procedures. Documentation will be on your company letterhead, as required by code. MATCO will arrange for full testing and evaluation of the welded test plates, including chemical, physical and non-destructive means of study. Typical means of testing:

  • Radiographic, ultrasonic, magnetic particle, dye penetrant inspection.
  • Microscopic and metallurgical examination.
  • Corrosion and stress-corrosion testing.
  • Tensile tests, bend tests, charpy impact tests and hardness tests.
  • Prepare Procedure Qualification Records (PQR's) and Weld Procedure Specifications (WPS's).

 

2. Welder Testing

MATCO can provide a full-time welding engineer at your facility to test welders to the applicable code. Test plates will be evaluated by destructive and/or non-destructive methods.Results will be documented on your company letterhead as required by code.

3. Failure Analysis

MATCO can investigate weld or weld-related failures using state of the art techniques.Reports will be generated detailing failure causes and recommended means of prevention.

4. Vendor Audits

A. MATCO can provide personnel to conduct audits of vendors and/or sub-contractors regarding weld- related activities or projects. For instance, compliance with ISO 9000 could be ascertained.

Macroetch of a Weld Structure

Partial list of Services Available for Welded Components

  • Failure analysis of welded components
  • Corrosion failure analysis of welds and welded components
  • Metallography/On-site metallography
  • Hardness testing/On-site hardness testing
  • Microhardness testing-Vickers and Knoop
  • Macroetch inspection
  • Sensitization of austenitic stainless steels per ASTM A262
  • Sensitization of ferritic stainless steels per ASTM A763
  • Chemical analysis of base metals for weldability and selection of preheat and post heat temperatures
  • Mechanical testing
  • Scanning electron microscopy
  • Chemical analysis of weld deposits
  • Seven gage delta ferrite determination in 300 series stainless steel welds

MATCO looks forward to discussing your welding issues to see what might be done to rectify your real cusp type problem in the welding area.

We Value Our Customers... Throughout the years, we have noticed that much of our business comes from repeat customers. Our expertise and well-equipped lab can account for much of this, but we believe there is something more to it. We attribute it to the fact that we promote an open and friendly environment that is never too busy to meet your needs. At MATCO, we value your business whether you are a large corporation or a small enterprise. We will provide you with the attention you need and deserve. We invite you to visit us and get to know our staff, and share in the learning experience.

Why Choose MATCO Services? As one of the premier testing and failure analysis firms featuring state of the art equipment, MATCO Services is able to provide a unique and diverse blend of services. Thousands of investigations have been performed at MATCO Services, ranging from jet engines and boiler tubes, to computer components and implants. Projects are not only conducted on your schedule from initiation to completion with competent and experienced personnel, and conducted in a discrete manner that ensures confidentiality as well.

 

Typical Projects

Although MATCO's work is vital to its clients, it is rarely seen by the public. Here are some examples of recent jobs in which MATCO provided the timely, competent, customer-oriented engineering analysis that made the difference.

Failure Analysis: Metallurgical support for a major commercial airline fleet (US Airways) that includes failure analysis investigations, corrosion investigations, and quality control testing. Bridge and construction failure investigations are routinly performed at MATCO

Corrosion Engineering: Cathodic protection system design and installation for a submerged ocean tunnel for the off-loading facility of the largest liquified natural gas (LNG) process facility in the United States . Our certified team of corrosion investigators can perform testing to evaluate the integrity of pressure vessels. These include refineries, underground and above ground oil, gas and chemical process facilities Our team has performed such analyses nation and worldwide, and will travel to your project site at a moments notice for emergency evaluations.

Paint/Coating Analysis: On-site and laboratory investigation of paint delamination failures (flaking and peeling) on galvanized structural members of several major stadiums in the United States .

On-site Inspection: Our certified team of inspectors can perform non-destructive testing on project sites to evaluate the integrity of large structures. Our team has performed such analyses nation and worldwide, and will travel to your project site at a moments notice for emergency evaluations. Such large structure evaluations have included off-shore oil platforms, wind power generation towers, concrete domes and stadiums, large underground cooling systems, and large elevated water towers. Our projects have taken us from Aloha Stadium in Hawaii to Alyeska Ski Resort in Alaska; from bridges in the Bahamas to titanium structures in Tokyo, Japan and damage evaluation of hurrican in Florida. This project included roofing, siding, paint and internal water damage for a large structure.

Enviromental Testing: Comparative testing of the resistance of pharmaceutical labels to environmental stresses (MFG, Humidity, and QUV testing) for a major drug company to determine what labels held up the best.

Fire Investigation: Same-day analysis of the effects of a truck fire on the superstructure of a major highway bridge to determine whether or not the highway could remain open.

Explosion Investigations: Failure analysis of a gas main explosion that caused casualities.

Power Plants: Failure analysis and remaining life determination of boiler components in the power industry.

Implant Materials: Electrochemical corrosion evaluation and failure analysis of implant materials such as hips, knees, stents, etc. to improve products and performance.

Galvanized Steel: How its microstructure and galvanized layer chemistry affect its appearance and corrosion resistance. Prevention and evaluation of storage rust, cracking of galvanized layer, failure of painted galvanized steel. Cabinet salt spray testing, EIS testing of painted galvanized steel and metallurgical characterization tests are routinly performed for galavanized and painted galvanized steel panels.

Utility and Light Poles & Lattices: Inspection and evaluation of galvanized, corten and painted carbon steel utility, light poles/lattices. Failure analysis, fatigue investigations, protective coating evaluation, life expectancy determination, corrosion evaluation, underground, ground level and above ground were included in this investigations

R&D: Research & Development of new materials, coatings and sensors for the pipeline, construction/chemical industry.

Failure Analysis Team

Our team is comprised of certified and experienced personnel from a variety of technical disciplines including: mechanical engineering, cathodic protection, paint inspection, chemistry, metallurgy, and materials science. We also have a vast array of laboratory and field testing equipment. All of MATCO's testing equipment is calibrated on a routine basis in accordance with both national and international standards, and is ready to be put to use at a moment's notice.

Our team includes professional engineers, mechanical engineers, chemists, coating specialists and NACE Certified Materials Selection/ Design / Corrosion/Coating Specialists (*) includes:

Dr. M. Zee(*) Mr. Geoff Rhodes (*)

Dr. Don Gibbon Mr. Kevin Groll (*)

Dr. George Bayer Ms. Debra Riley (*)

Mr. Joe Tureck Mr. Ed Larkin

Mr. Ed MaCan, PE Mr. Walter Gretz, PE

Dr. Kasraie, PE Dr. Huping Xue

Dr. Bavarian Mr. Jay Metha

An illustrated formal report documents the results of the investigation. If necessary, MATCO personnel can usually be on site almost immediately when requested during emergency situations.

Failure Analysis

  • Identificaiton of Types of Failures
  • Ductile and Brittle Factures
  • Fatique Failures
  • Distortion Failures
  • Wear Failures
  • Liquid Erosion Failures
  • Corrosion Failures
  • Stress Corrosion Cracking
  • Liquid Metal Embrittlement
  • Embrittlement by Solid Metal Environments
  • Hydrogen Damage Failures
  • Corrosion Fatique Failures
  • Elevated Temperature Failures
  • Failures in Sour Gas Environments

Types of Failures Dealt with on a Routine Basis

  • Failures of Cold Formed Parts
  • Failures of Forgings
  • Failures of Iron Castings
  • Failures of Steel Castings
  • Failures of Weldments
  • Failures of Brazed Joints
  • Failures of Shafts
  • Failures of Sliding Bearings
  • Failures of Rolling Element Bearings
  • Failures of Lifting Equipment
  • Failures of Mehcanical Fasteners
  • Failurs of Springs
  • Failures of Tools and Dies
  • Failures of Gears
  • Failures of Boilers and Related Equipment
  • Failures of Heat Exchangers
  • Failures of Pressure Vessels
  • Failures of Metallic Orthopedic Implants
  • Failures of Pipelines
  • Failures of Bridge Components
  • Failures of Locomotive Axles
  • Failure Analysis of Continuou Fiber Reinforced Composites
  • Failure Analysis of Ceramics
  • Failure Analysis of Polymers
  • Failure Analysis of Integrated Circuits
  • Concrete cracking and Petrographic Analysis
 


The Next Step... While Matco Services' has the expertise and the technology to unravel even the most difficult material failures, your input is vital for a complete analysis. By filling out the service request form and giving us a description of the problem, you can be sure that all aspects of your problem will be considered. We'll send you a proposal for your work, including methods and costs.

Matco Services' Contact Information:
email: info@matcoinc.com

Matco Services, Inc. – Pittsburgh Main Headquarters:
100 Business Center Drive,
Pittsburgh, PA 15205

Toll Free: (800) 221-9090
Telephone: (412) 788-1263

Florida Office Address:
Matco Services, Inc.
4131 SW 47th Ave., Suite 1407 (New Town Commerce Center)
Davie, FL 33314

Telephone: (954) 797-6863

Omaha Office Address:
Matco Services, Inc.
7002 North 288th,
Valley, NE 68064 USA

Telephone: (877) 359-6114