The word polymer comes from the Greek polumeres which means “having many parts”. Polymers are large molecules consisting of repeated chemical units (“mers”) joined together, usually in a line, like beads on a string. Each “mer” is typically made up of more than 5 and less than 500 atoms. The word “polymer” is applied when you have more than about 50 “mers” strung together.

Even though the basic makeup of many polymers is carbon and hydrogen, other elements can also be involved. Oxygen, chorine, fluorine, nitrogen, silicon, phosphorous, and sulfur are other elements that are found in the molecular makeup of polymers. Polyvinyl chloride (PVC) contains chlorine. Nylon contains nitrogen. Teflon contains fluorine. Polyester and polycarbonates contain oxygen. There are also some polymers that, instead of having a carbon backbone, have a silicon or phosphorous backbone. These are considered inorganic polymers. One of the most famous silicon-based polymers is Silly Putty.

The joining of small molecules to produce large molecules in a chemical reaction is called polymerization. The main polymerization processes in polymers are addition (chain reaction) polymerization and condensation (step reaction) polymerization. The addition process is the simpler of the two. By use of heat and pressure in an autoclave or reactor, double bonds of unsaturated monomers break open and then link to form chains. These addition reactions are atoms or groups of atoms that attach themselves to the carbon atoms at the sites of multiple bonds. No products other than the polymer are formed. Saturated hydrocarbons undergo substitutional reactions in which hydrogen atoms are replaced by other atoms or groups of atoms. The products of addition polymerization or chain reaction polymerization include polypropylene (PP), polyethylene (PE), poly(vinyl acetate) (PVA), poly(vinyl chloride) (PVC), acrylonitrile-butadiene-styrene (ABS), and polytetrafluoroethylene (PTFE). Addition polymers generally fit into the thermoplastic (soften when heated) group.

Most plastics that cannot be resoftened when heated (thermosetting polymers) come from condensation polymerization, also known as step reaction polymerization. This group gets its name from the by-product (condensate) of the polymerization, which is often water, but it may be a gas. Phenolic (PF), polyester (PET), silicon (SI), and urethanes (PUR) are typical thermosets from the step reaction synthesis, while nylon (PA) and polycarbonates (PC) are thermoplastic resins synthesized through step polymerization.

Polymer Clasification

Polymers are classified according to similar molecular architecture rather than similar chemical structures. There are three classes of polymers: rubber, thermoplastics, and thermosets. Thermosets are rigid crosslinked polymers where once heated or cured, they cannot be reheated again or they will degrade.

When a thermoplastic material is heated and pressed into a mold, no chemical reaction of any kind takes place. Once the plastic has cooled and hardened in this shape, it could be reheated and remolded without any perceptible change in its properties. An example of this is ice.

Thermoplastics

Thermoplastics have some degree of structural stability even though the chains are not crosslinked or bonded together by covalent bonds. Thermoplastics can be linear or branched and amorphous or crystalline. Their use temperature must be below the glass transition temperature or the crystallization temperature or else the thermoplastic will flow.

Thermoplastics have one or more of the following twelve (12) items added to improve properties: reinforcing agents, fillers, coupling agents, stabilizers, pigments, dyes, plasticizers, lubricants, processing aids, curing agents, blowing agents, and flame retardants. Stabilizers are added because most polymers are susceptible to one (1) or more forms of degradation as a result of environmental exposure to O2 or UV or high temperature. Stabilizers inhibit degradation. With the proper stabilizer, the heating and cooling cycles can be repeated many times as long as the heating temperature is less than the polymer degradation temperature.

Thermosets

Thermosets, on the other hand, do undergo chemical change while they are being formed. They react by polycondensation and cross-link to form a three-dimensional lattice. This type of curing produces a structural change of the molecules, which is irreversible. Crosslinking is initiated by heat, light, or the addition of other chemicals. It is not a reversible process resulting in materials, which cannot be recycled. Once a thermoset has achieved its final shape, it cannot be reformed. Examples of thermosets are an egg and epoxy glue.

Thermoset polymers have covalent bonds linking the polymer chains in three dimensions. These links prevent the chains from sliding past one another resulting in a higher modulus and improved creep resistance. Usually thermosets are more brittle than thermoplastics.

Elastomers

Elastomers are long polymer chains, usually lightly crosslinked, and are easily deformed. Common elastomers include polybutadiene (used in shoe soles), polyisobutylene (used in automobile tires), and polyisoprene (natural rubber).

Elastomeric polymer chains can be crosslinked, or connected by covalent bonds. This process is sometimes called vulcanization. Crosslinking is initiated by heat, light, or the addition of chemicals. Note that thermosets are similar to elastomers. The polymer chains in thermosets are below their glass transition at room temperature, making them glassy. In contrast, the polymer chains in elastomers are above their glass transition at room temperature, making them rubbery.

Crosslinking makes elastomers reversibly stretchable for small deformations. When stretched, the polymer chains become elongated and ordered along the deformation direction. This is entropically unfavorable, which is opposite for a metallic spring. When no longer stretched, the chains randomize again. The crosslinks guide the elastomer back to its original shape.

 


The Next Step... While Matco Services' has the expertise and the technology to unravel even the most difficult material failures, your input is vital for a complete analysis. By filling out the service request form and giving us a description of the problem, you can be sure that all aspects of your problem will be considered. We'll send you a proposal for your work, including methods and costs.

Matco Services' Contact Information:
email: info@matcoinc.com

Matco Services, Inc. – Pittsburgh Main Headquarters:
100 Business Center Drive,
Pittsburgh, PA 15205

Toll Free: (800) 221-9090
Telephone: (412) 788-1263

Florida Office Address:
Matco Services, Inc.
4131 SW 47th Ave., Suite 1407 (New Town Commerce Center)
Davie, FL 33314

Telephone: (954) 797-6863

Omaha Office Address:
Matco Services, Inc.
7002 North 288th,
Valley, NE 68064 USA

Telephone: (877) 359-6114