Matco's Tecnical Notes
A Re-Examination of Failure Analysis, by Dr. Mehrooz Zamanzadeh, Dr. Donald Gibbon, and Edward Larkin, internally published by Matco Associates
Failure Analysis of Coatings, by Dr. George T. Bayer and Dr. Mehrooz Zamanzadeh, Internally published by Matco Associates
Cathodic Protection, by Dr. Zee, Dr. Gibbon, Geoff Rhodes and Dr. George Bayer, Internally published by Matco Associates
Some Failure Analysis Case Histories in Galvanized Steel Products , M. Zamanzadeh and Ed Larkin internally published by Matco Associates
Discovering Outgassing Defects, M. Zamanzadeh, internally published by Matco Associates
Evolution of Material Analysis, Dr. Gibbon, internally published by Matco Associates
Modeling Robotic Failure by FEA, Dr. Zamanzadeh, internally published by Matco Associates
Polymer Science 101, internally published by Matco Associates
High Temperature Corrosion, internally published by Matco Associates
DNA Sequencing to Pinpoint Corrosion-Causing Bacteria in Steel , Materials Performance, March, 2004
Label Testing for Pharmaceuticals , US Pharmacist, in press Case Study of Complex Pitting Corrosion on 316L Stainless Steel Condenser Tubing: The Roles of Bacteria, Metallurgy and Water Chemistry. International Water, Journal of IWC, vol. 1, issue 2, pp 2-8, w. Wiatr and McGough
Chemical Composition, Electrochemical and Morphological Properties of Iron Phosphate Conversion Coatings, Corrosion, vol. 55, #9, pp 898-906, w. Warburton, Jackson, Gate, Rodnysansky and Warburton.
Chemical and Mechanical Damage to Paper Machine Felts: A Review , presented at the 2000 Papermakers Conference, Vancouver , British Columbia , and published in the Conference Proceedings.
How Roebling Did It: The Building of the Worlds First Wire Rope Suspension Aqueduct in Pittsburgh of the 1840's, to be presented at Materials Science & Technology Conference, Pittsburgh, PA.

|
The Next Step... While Matco has the expertise and the technology to unravel even the most difficult material failures, your input is vital for a complete analysis. By filling out the service request form and giving us a description of the problem, you can be sure that all aspects of your problem will be considered. We’ll send you a proposal for your work, including methods and costs. Solutions are just around the corner!
Join us at www.materialsforum.com to discuss the hottest topics in corrosion, failure analysis, paint & coatings, concrete (petrography) testing, materials testing, and more. The Materials Forum provides you the opportunity to ask questions and get feed back from our qualified and experienced staff engineers. We look forward to hearing from you!
Matco Contacts for Main & Florida Offices: Toll-Free: 1-800-221-9090 Matco Main: (412) 788-1263 Matco Florida: (954) 563-6440 Emergency Contact: (412) 952-9441
email: info@matcoinc.com
Main Office Address: Matco Associates, Inc. 4640 Campbells Run Road Pittsburgh, PA 15205
Florida Office Address (Serving the Miami, Ft. Lauderdale, Orlando, Tampa, Daytona, and Jacksonville Areas): Matco Associates, Inc. 4131 SW 47th Ave., Suite 1407 (New Town Commerce Center) Davie, FL 33314
|
|
|