Towers, Poles, Lattice & Anchor Rod Inspections
-
Transmission Tower Inspection
|
-
Pole/Lattice Tower Inspection
|
-
Communication Tower Inspection
|
-
Pole/Lattice Integrity Assessment
|
-
Corrosion Inspection and Analysis
|
-
Failure Investigations & FEA Analysis
|
-
Cathodic Protection Inspection
|
-
Anchor Rod Inspection and Failure Analysis
|
-
Non-Destructive Inspection
|
-
Evaluation of Pack Out (Corrosion Build-up)
|
-
Paint and Coating Inspection
|
-
Technical Audit of Galvanized Pole & Lattice Plants
|
-
Remaining Life Estimations
|
|
-
Quality Control Inspection
|
-
Computerized On-Site Inspections
|
|
|
-
Visual On-Site Inspections
|
-
Hurricane Damage Evaluation
|
|
The objective for the inspection and assessment is to gather data and provide information necessary to address the following issues and:
1. Ensure integrity and safety
2. Determine corrosion rate and life expectancy
3. Forecast and plan maintenance
4. Extend life of the systems
5. Achieve safety, integrity, and service life at a minimum cost
Matco Associates, Inc. will initialy assess the towers by completing soil resistivity measurements directly on-site at different depths, therefore including the entire underground portion (including the water table, if present). The electrochemical potential measurements will identify lattice legs, anchor rods or poles are corroded to the steel surface (i.e. the sacrificial galvanized zinc layer have been consmed partially or entirely). The results will indicate if cathodic protection should be installed immediately to prevent further corrosion of the component. The electrochemical corrosion rate determination will provide further information on the life expectancy of the structure and plan future maintenance guidelines. More accurate measurement of the soil resistivity will also indicate the quality of the grounding system.
* Visual examination of above grade portions of towers,poles, ground anchors and CP assets; include appropriate digital photographic documentation.
* Electrochemical measurements at towers, poles and each ground anchor which will immediately indicate the genertal corrosion activity and identify any hot spots or areas of extreme corrosion.
* Excavation the backfill soil to a depth of three feet to allow for visual examination and thickness measurement on the ground anchors or tower legs.
* On-site soil resistivity measurements at three different depths, depending on the depth or design of the given tower.
* On-site determination and documentation of the moisture content of the soil.
*On-site determination and documentation of the chloride/sulfate/sulfide.. concentration.
In Matco's approach the testing will be in accordance with American Society for Testing and Materials (ASTM) standards and American Association of State Highway and Transportation Officials (AASHTO) standars. The testing will be perfomed by certified technicians and reviewed by a NACE Certified Corrosion and/or Cathodic Protection Specialist.
Matco Associates has years of experience in all aspects of on-site and laboratory inspection and assessment of utility and traffic poles plus lattices and transmission towers. Our team includes Ph.D.s, registered professional engineers, and certified inspectors from a variety of technical disciplines, including mechanical engineering, paint inspection, chemistry, metallurgy and materials science. We also have a comprehensive array of laboratory and field testing equipment, all calibrated on a routine basis in accordance with both national and international standards. This team is ready to be put to use at a moment's notice for inspection and investigation of:
1-Galvanized and Cor-ten Utility Poles and Transmission Lattice Towers
2-Galvanized and Cor-ten Traffic and High Mast Lighting Poles
3-Alumnium Traffic and Light Poles
Corrosion on transmission-line towers and poles is directly related to the atmospheric and soil conditions present for the unique location of a given pole structure, as well as to the materials of manufacturing and the quality of these materials.
1-Internal corrosion due to the presence or entrapment of corrosive water (electrolyte)
2-External corrosion due to corrosive atmospheric and environmental conditions
3-Fatigue of Traffic and Light Poles due to wind loading and inadequate design
4-Manufacturing defects and improper paint coating selection and application
5-Little or no maintenance in corrosive environment
6-Accumulation of debris and soil under base plate
Internal Corrosion and Perforation of a Cor-ten Pole in an Deicing Salt Containing Environment
Transmission Towers and Galvanized Utility Poles
Towers in submerged conditions are subject to a greater risk of corrosion because of the continuous presence of moisture – the electrolyte necessary to have the electrochemical corrosion reaction proceed. The specific chemical composition, resistivity and redox potential of the electrolyte in the soil will determine the relative corrosivity or risk of corrosion.
In addition to the soil characteristics, it is useful to measure the electrochemical potential of the structure in the electrolyte. This is done using methodologies developed by the underground pipeline industry and recognized by NACE International and other professional societies and regulatory organizations. The structure-to-soil potential of a buried asset can be related to the present state of corrosion, with less electronegative values of potential indicated an increasing likelihood of active corrosion. By using sacrificial (galvanic) cathodic protection, corrosion can be mitigated by shifting the structure-to-soil potential to more electronegative values where the corrosion reactions are not favored thermodynamically. The amount of galvanic current required to obtain acceptable levels of cathodic protection can be calculated.
Close up picture of Pack Out (Corrosion Product Built up) in a Cor-Ten Steel Transmission Tower.
Note deformation and bending of joint plate
A site investigation includes partial excavation for visual assessment of the underground structure. The visual observation complements the non-invasive structure-to-soil potential evaluation and, in the instances of active corrosion, allows direct assessment of the state of corrosion and material loss. It also allows for visual observation of mechanical damage (bent components) and the condition of protective coatings at and below the ground line. If sufficient material loss has occurred to compromise the design strength of the structure, replacement of the components may be required.
Matco's extensive experience with painted and unpainted galvanized steel towers provides specific knowledge and know-how that can evaluate these structures from the coating point of view, the first defense against corrosion in these structures. We can evaluate the existing coating, predict its performance both under and above ground, and also recommend repair or select a new coating for that specific soil application. This knowledge comes from our experience in evaluation of numerous coated galvanized transmission structures in different soil environments and atmospheric conditions. This type of evaluation requires both metallurgical and polymer coating experience with painted galvanized steel. Very few firms have the specific knowledge required to evaluate aged painted galvanized towers and poles.
The first steps in a site investigation for transmission towers include recording the tower identification, type, and GPS location. Leg orientation will be confirmed and recorded before performing any inspection evaluations. The immediate area surrounding the structure must also be examined and documented to look for other structures or buried assets which may influence the evaluations which are to follow.
Soil resistivity will first be measured and recorded as specified at each leg of the structure before any soil is disturbed. Structure-to-soil potentials will also be profiled at each leg before soil disturbance. The profile length should equal the reported depth of the sub-surface structure. To the extent possible the profile should proceed radially away from the leg corner in order to minimize potential gradient influence from the adjacent legs.
As excavation proceeds, soil samples should be obtained from the near-surface and bottom of the excavation, or wherever different soil conditions are noted. Soil pH and redox potential should be measured on-site; samples will be procured for off-site analyses of sulfur and chloride content, with enough sample quantity retained for additional evaluations of pH, soil composition or soil resistivity per ASTM G 57 if required or requested at a later time.
Excavation of the buried structure to the required depth should be conducted. Dirt/rust removed should be removed from the structure by brushing and/or washing. Visual assessment may be complemented by holiday testing on coated structures; paint and zinc coating thickness measurements may both be required.
Fatigue of Traffic and Light Poles
Most pole designs prior to 2001 are suspect for fatigue cracking because the design procedures did not considered cyclic loading due to fatigue. Pole structures should be designed so that the stress ranges due to the fatigue design wind loads are less than the fatigue thresholds for each detail, thus ensuring that fatigue will not occur even for a large number (hundreds of millions) of wind load cycles. In the Aashto 2001 Specification, the fatigue design procedures are based on control of the nominal stress range and knowledge of the fatigue threshold of the details. Each of these details is assigned a "Stress Category" and the fatigue threshold stress range for each category is given for this Specification.
If traffic poles are suspected of having crack(s), or if there have been catasrophic failures of the at the weld toe locations in the past, poles with the same design at a project site should be evaluated by ultrasonic testing or other forms of non destructive testing methods to identify additional suspect poles. MATCO highly recommends that all similar pole structure be inspected immediately and that cracked poles be taken out of service as soon as possible. There is only a small window of time when the cracks are both large enough to detect, and small enough to not yet cause catastrophic failures. In most cases improper design and selection of poles play an important factor in ultimate failure. Fatique cylic loads, vibration and wind loading should be consider for the design. wind Matco can establish a program to inspect the poles with similiar design for fatigue cracking.
Fatigue cracks at the toe of the weld is shown in top Photo for a galvanized pole.The bottom photo exhibits the catasrophic failure of the pole. It should be noted that there is only a small window of time when the cracks are both large enough to detect, and small enough to not yet cause catastrophic failures.
Design calculations should be prepared and stamped by a professional engineer explicitly showing the fatigue design as well as the traditional allowable stress design for strength.
Corrosion Failures -The investigation of pole corrosion failures can be complex, and usually requires multidisciplinary testing and analysis to determine the root cause of failure. The end determination must be able to be made with a high degree of certainty to ensure that proper design , replacement materials or adequate coatings are selected and that the most effective corrosion control methods are used. Experience is surely the most important ingredient to look for when choosing a materials firm to handle your corrosion control and failure analysis needs. We like to cite few examples:
Electrochemical Cell for Evaluation of Corrosive soil and Trapped Water. The electrochemical corrosion testing will provide information on corrosion rate in mills/year(mpy) and whether or not the soil is reducing (i.e. the corrosion rate will increase with time)
Corrosion Protection For Poles:
Pole structures that are to be stored prior to use should be protected from moisture retention and kept well ventilated. Immediate removal of all packing and shipping materials is recommended to prevent accelerated finish deterioration. A good stock rotation program (first in – first out) is recommended to minimize storage damage or deterioration. Foundation details should assure that water or excessive moisture cannot accumulate at the base of the pole. This includes providing drainage for any water caused by condensation inside the pole.
Lack of drainage for water may result in acclerated corrosion
All finishes are subject to gradual deterioration. The rate of deterioration is a function of many variables such as:
-
Ultraviolet damage from constant sun exposure
-
Corrosive elements in the atmosphere.
-
Ground level exposure to mechanical damage.
-
Salt spray from road surfaces, or a marine environment.
-
Ground level exposure to corrosive materials and soil conditions.
-
Moisture from rainfall or condensation
-
Underground soil / ground water exposure
On-site Inspection & Investigations -Our certified team of inspectors can perform non-destructive testing on project sites to evaluate the integrity of pole and lattice structures. Our team has performed such analyses nation and worldwide, and will travel to your project site at a moments notice for emergency evaluations. Such large structure evaluations have included off-shore oil platforms, wind power generation towers, concrete poles, galvanized poles, cor-ten and alumnium poles, paint systems for c.steel and galvanized poles, and large elevated wind towers. Our projects have taken us from chicago, california, Pennsylvania, Hawaii to Alaska; from poles in Tennesse to Cor-ten poles in Chicago, IL.
We know that the most common failure modes for light poles is internal corrosionfrom build-up of moisture inside the pole, external corrosion due to deicing salts, and fatigure fracture from cyclic wind loading. Depending on complexity of project, on-site investigation and test protocol may include any or all of the following:
-
Description of pole installation including the base plate and weld toe examination for corrosion attack, cracks and photo-documentation of the project site
-
Ultrasonic wall thickness measurment and thickness loss determination
-
Non-destructive testing of the weldment at the base plate/pole connection
-
Review of design, engineering and fracture mechanics calculations
-
Evaluation of paint system (determination of thickness of paint layers, adhesion and % protection)
-
Sampling of peeled paint and corrosion products for further laboratory examination
-
Failure mode determination and determination of root cause
-
Life expectancy determination
-
Recommendations and determination of inspection frequency
If necessary, Matco personnel can be on site almost immediately when requested during emergency situations. An illustrated formal report documents the results of the investigation.
Other Matco's Services
The Matco team has experience working in many other diverse fields; from fracture mechanics, cathodic protection to paint inspection to failure analysis to remaining life determination. Some of our clients include Allegheny Energy, Valmont, California Edison, US Airways, First Energy and NY Power.
Corrosion Engineering & Failure Analysis
Experienced PE, PhD Scientists, NACE Certified in Corrosion, Coating, Design , Materials Selection & Cathodic Protection Specialists who will solve your corrosion problems at both initial design stages and in service. Matco provides corrosion evaluation and failure analysis investigations for : (a) underground facilities (b) above ground facilities and (c) strcutres in marine environments. Matco can investigate corrosion or corroso -related failures using state of the art techniques.Reports will be generated detailing corrosion failure causes and recommended means of prevention.
-
Corrosion evaluation, life expectancy determination and cathodic protection of underground pipe lines, water mains, electrical poles and transmission lattices
-
Corrosion mapping, detection of "Hot Spots", cathodic protection of reinforced concrete structures
-
Coating/Paint Investigations
-
Electrochemical EIS , DC and AC Testing - Determination of cathodic protection criteria for non-ferrous alloys and stainless steels
-
On-site Evaluation of tanks and corrosion mitigation by protective coatings and internal or external Cathodic Protection
-
Corrosivity determination of soil, water and determination of corrosion mitigation techniques
-
On-site coating evaluation and selection of coatings for specific corrosive environments by EIS
Our team includes NACE Certified Corrosion / Cathodic Protection / Materials Selection / Design / Coating Specialists (*)and other materials experts includes:
Dr. M. Zee(*) Mr. Geoff Rhodes (*)
Dr. Don Gibbon Mr. Kevin Groll (*)
Dr. George Bayer Ms. Debra Riley (*)
Mr. Gordon Kirkwood Mr. Ed Larkin
Dr. Kasraie Dr. Bavarain
Related Recent Publications:
Painted Galvinized Steel Case HIstories, by Dr. Mehrooz Zamanzadeh, Dr. George Bayer, and Gordon Kirkwood, presented at PACE Conference 2006.
Laboratory and Field Corrosion Investigation of Galvanized Utility Poles, by M. Zamanzadeh, C. D. Kempkes, D. Aichinger and D. Riley
A Re-Examination of Failure Analysis, by Dr. Mehrooz Zamanzadeh, Dr. Donald Gibbon, and Edward Larkin, internally published by Matco Associates, Inc.
Failure Analysis of Coatings, by Dr. George T. Bayer and Dr. Mehrooz Zamanzadeh, internally published by Matco Associates, Inc.
Painted Galvinized Steel Case HIstories, by Dr. Mehrooz Zamanzadeh, Dr. George Bayer, and Gordon Kirkwood, presented at PACE 2006.
Final Words
We Value Our Customers... Throughout the years, we have noticed that much of our business comes from repeat customers. Our expertise and well-equipped lab can account for much of this, but we believe there is something more to it. We attribute it to the fact that we promote an open and friendly environment that is never too busy to meet your needs. At Matco, we value your business whether you are a large corporation or a small enterprise. We will provide you with the attention you need and deserve. We invite you to visit us and get to know our staff, and share in the learning experience.
Why Choose Matco Associates? As one of the premier testing and failure analysis firms featuring state of the art equipment, Matco Associates is able to provide a unique and diverse blend of services. Thousands of investigations have been performed at Matco Associates, ranging from jet engines and boiler tubes, to computer components and implants. Projects are not only conducted on your schedule from initiation to completion with competent and experienced personnel, and conducted in a discrete manner that ensures confidentiality as well.

|
The Next Step... While Matco has the expertise and the technology to unravel even the most difficult material failures, your input is vital for a complete analysis. By filling out the service request form and giving us a description of the problem, you can be sure that all aspects of your problem will be considered. We’ll send you a proposal for your work, including methods and costs. Solutions are just around the corner!
Join us at www.materialsforum.com to discuss the hottest topics in corrosion, failure analysis, paint & coatings, concrete (petrography) testing, materials testing, and more. The Materials Forum provides you the opportunity to ask questions and get feed back from our qualified and experienced staff engineers. We look forward to hearing from you!
Matco Contacts for Main & Florida Offices: Toll-Free: 1-800-221-9090 Matco Main: (412) 788-1263 Matco Florida: (954) 563-6440 Emergency Contact: (412) 952-9441
email: info@matcoinc.com
Main Office Address: Matco Associates, Inc. 4640 Campbells Run Road Pittsburgh, PA 15205
Florida Office Address (Serving the Miami, Ft. Lauderdale, Orlando, Tampa, Daytona, and Jacksonville Areas): Matco Associates, Inc. 4131 SW 47th Ave., Suite 1407 (New Town Commerce Center) Davie, FL 33314
|
|
|